Abstract

The importance of hydrochloric and sulfuric acids to the chemical process industries cannot be overstated. There has always been a desire for materials with improved resistance to these two acids, without the drawbacks associated with the nickel-molybdenum alloys. The Hybrid-BC1 alloy is significantly more resistant to HCl and H2SO4 than the Ni-Cr-Mo alloys and additionally, is resistant to oxidizing chemicals in the acid that are very detrimental to B-Family alloys. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-679. Producer or source: Haynes International Inc.