Abstract

HPM 80/20A and HPM 80/20AL are resistance alloys used in electric heating elements. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming. Filing Code: Ni-631. Producer or source: Hamilton Precision Metals.