Incotherm TD is a thermocouple-sheathing alloy with elements of silicon and rare earths to enhance oxidation resistance at high temperatures. This datasheet provides information on composition, physical properties, and tensile properties as well as deformation. It also includes information on high temperature performance and corrosion resistance as well as forming. Filing Code: Ni-628. Producer or source: Special Metals Corporation.