Sandvik Sanicro 75X1 is a nickel-base age-hardenable spring wire. This datasheet provides information on composition, physical properties, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-627. Producer or source: Sandvik Steel Company.