Nicrobraz 31 is a high-chromium, oxidation-resistant nickel braze filler metal with enhanced flow properties. This datasheet provides information on composition. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-614. Producer or source: Wall Colmonoy Corporation.