RIMA 625, or 62-50, is a consumable or solid wire for tungsten inert gas (TIG), metal inert gas (MIG), and submerged arc welding (SAW). The consumable is used for matching the nickel-base alloy 625 or N06625 (see Alloy Digest Ni-121, February 1967) with typical composition Ni-20%Cr-9%Mo-3.5%Nb. The product is also used as an overmatched product with respect to corrosion resistance for alloys 825, G, G3, Alloy 28, 904L and the 6% Mo group of materials. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as machining and joining. Filing Code: Ni-599. Producer or source: Metrode Products Ltd.