RIMA HAS C22 is a Ni-Cr-Mo-W-type consumable with a nominal composition of Ni, 22% Cr, 13.5% Mo, and 3% W, and it is used to join high-molybdenum-containing corrosion-resistant alloys to themselves and each other by tungsten inert gas (TIG) welding. This datasheet provides information on composition, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating and joining. Filing Code: Ni-592. Producer or source: Metrode Products Ltd.