Abstract

Rima 617 is an Inconel-type consumable with a nominal composition of Ni, 24% Cr,12% Co, and 9% Mo and is used to join UNS N06617 and Nicrofer 6023 to themselves. The alloy is designed for high-temperature service and is often used as the weld metal in dissimilar cases to ensure the weld has as good strength as does the base metal. Tungsten inert gas (TIG) wire for this alloy is referred to as 61-70. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on joining. Filing Code: Ni-590. Producer or source: Metrode Products Ltd.