NimRod C276 and C276KS are Ni-Cr-Mo-W-type welding consumables with a nominal composition of Ni, 15% Cr, 16% Mo, 4% W, and 5% Fe. They are used to join high-molybdenum-containing corrosion-resistant alloys to themselves and each other. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: Ni-589. Producer or source: Metrode Products Ltd.