Abstract

RA602CA has a high creep rupture strength with alloying additions of titanium, zirconium, and high carbon. High chromium combined with aluminum and yttrium give the alloy a tight oxide scale and good cyclic oxidation behavior. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-586. Producer or source: Rolled Alloys Inc.