Abstract

Incocal Alloy 10 is a direct melt additive alloy of nickel with calcium to scavenge deleterious elements and improve ambient and high-temperature properties of both iron- and nickel-base alloys. This datasheet provides information on composition and physical properties. Filing Code: Ni-576. Producer or source: International Nickel Inc.