Abstract

UCI-471 is an improved version of the HP classification of furnace tube alloys with better oxidation and creep resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-562. Producer or source: Ultra-Cast Inc.