Abstract

Nicrobraz 110 is a low-melting brazing filler metal with improved corrosion resistance for applications requiring high joint strength and oxidation resistance up to 2200F. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining and powder metal forms.Filing Code: Ni-522. Producer or source: Wall Colmonoy Corporation.