Abstract

ANVAL 625 is a corrosion- and oxidation-resistant coating superalloy. Applications include the restoration of equipment for the pulp and paper, chemical process, and gas turbine industries. This datasheet provides information on composition, physical properties, and hardness. It also includes information on machining, surface treatment, and powder metal forms. Filing Code: Ni-519. Producer or source: ANVAL.