Nicrofer 7216 is a nickel-chromium-iron alloy, with good resistance to oxidation, carburization, and nitriding; good resistance to stress-corrosion cracking; and good resistance to dry chlorine and hydrogen chloride. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-518. Producer or source: VDM Technologies Corporation.