Hastelloy C-2000 has a broad capability range for handling corrosive environments. The alloy has high resistance to reagent grade sulfuric acid, hydrochloric acid to high concentrations, and nitric acid. The alloy has outstanding localized corrosion resistance, excellent stress-corrosion cracking resistance, and good thermal stability. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-516. Producer or source: Haynes International Inc.