Abstract

COLMONOY No. 83 PTA is a nickel-base hard surfacing alloy containing tungsten carbide. The application method is plasma transferred arc and the application is designed to protect extrusion screws. This datasheet provides information on composition, physical properties, microstructure, hardness, tensile properties, and compressive strength. It also includes information on wear resistance as well as machining and powder metal forms. Filing Code: Ni-493. Producer or source: Wall Colmonoy Corporation.