Abstract

NICROFER 45 TM is alloyed with chromium, silicon, and rare earth additions to produce an alloy oxidation resistant, especially for applications such as waste incineration. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-477. Producer or source: VDM Technologies Corporation.