Abstract

CARLSON ALLOYS C 800/800H have good strength plus excellent resistance to oxidation and carburization at elevated temperatures. Fair degree of resistance to stress-corrosion cracking. They resist sulfur attack, internal oxidation, scaling and corrosion in industrial atmospheres. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: Ni-474. Producer or source: G.O. Carlson Inc.