NICROBRAZ 160 is for wide clearance joints where heavier fillets or greater joint ductility and machinability are desired. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-472. Producer or source: Wall Colmonoy Corporation.