Nicrofer 6616hMo is an austenitic low-carbon nickel-molybdenum-chromium alloy characterized by very good resistance to corrosive media under highly oxidizing conditions and by excellent resistance to crevice and pitting corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: Ni-465. Producer or source: VDM Technologies Corporation.