Abstract

NICROBRAZ 30 is used for well diffused, high strength, heat resistant joints, and highly stressed structures such as jet engine parts. It is also used in nuclear reactors where boron cannot be tolerated. It has low base-metal penetration. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-457. Producer or source: Wall Colmonoy Corporation.