Abstract

INCOLOY ALLOY 908 is a nickel-iron alloy developed for applications in the advanced TOKAMAK reactor ITER. The alloy contains no cobalt, a small level of chromium to resist stress assisted grain boundary oxidation (SAGBO) and is stabilized with Cb(Nb), Ti, and Al. This datasheet provides information on composition and tensile properties. It also includes information on heat treating. Filing Code: Ni-446. Producer or source: Inco Alloys International Inc.