Abstract

HASTELLOY alloy C-276 is a solid solution, nickel-molybdenum-chromium alloy, with outstanding resistance to localized corrosion and to both oxidizing and reducing media. (See Alloy Digest Ni-164, May 1971, for base metal.) This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-440. Producer or source: Haynes International Inc.