Abstract
DELORO 711 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance as well as machining and joining. Filing Code: Ni-431. Producer or source: Deloro Stellite Inc.