Abstract
NICROFER 5923 hMo, often called Alloy 59, was developed with extra low carbon and silicon contents and with a high alloy level of molybdenum to optimize its corrosion resistance. Nicrofer 5923hMo has a face-centered cubic structure. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-430. Producer or source: VDM Technologies Corporation.