Abstract

P/M LOW CARBON ASTROLOY offers good ductility and oxidation resistance in addition to excellent strength at high temperatures. This datasheet provides information on composition, physical properties, microstructure, and elasticity as well as creep. It also includes information on high temperature performance as well as heat treating. Filing Code: Ni-428. Producer or source: Crucible Compaction Metals.