INCONEL WELDING ELECTRODE 152 is a high chromium rod for shielded-metal-arc welding of Inconel Alloy 690 (Alloy Digest Ni-266, March 1981). Higher chromium is beneficial in resisting stress-corrosion cracking in high purity water for pressurized water reactors and for resistance to oxidizing acids. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-406. Producer or source: Inco Alloys International Inc..