Abstract

CRONIFER II EXTRA, 45, III EXTRA AND IV EXTRA alloys are high heat resistant alloys, some with resistance to green rot and hardening environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. Filing Code: Ni-405. Producer or source: VDM Technologies Corporation.