Abstract

HAYNES HR-160 alloy is a solid-solution-strengthened alloy with outstanding resistance to most forms of high-temperature corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-396. Producer or source: Haynes International Inc..