Abstract

INCONEL Filler Metal 82 is used for gas-tungsten-arc, gas-metal-arc, and submerged-arc welding of INCONEL alloys 600, 601 and 690, INCOLOY alloys 800 and 800H, and INCO alloy 330. It also is used for surfacing of steel. Dissimilar-welding applications for which the filler metal is used include joining INCONEL alloys, INCOLOY alloys and alloy 330 to nickel, MONEL alloys, stainless steels and carbon steels. It also is used to join stainless steels to nickel alloys and carbon steels. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-342. Producer or source: Inco Alloys International Inc..