PYROMET 751 is an age-hardenable nickel-base alloy with good stress-rupture properties to 1600 F. Its creep rate is low under high stresses at 1200-1500 F. It is highly resistant to chemical corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-335. Producer or source: Carpenter Technology Corporation.