Abstract

MONEL Filler Metal 60 is a nickel-base alloy used for gas-tungsten-arc, gas-metal-arc and submerged-arc welding of MONEL. alloys 400, 400, R-405 and K-500. It also is used for surfacing of steel. The weld metal deposited by Filler Metal 60 has properties similar to those of MONEL. alloy 400. It has good strength and resists corrosion in many media. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-321. Producer or source: Huntington Alloys.