Abstract

HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-317. Producer or source: Cabot Wrought Products.