INCONEL Welding Electrode 112 is a nickel-base alloy that is used for welding INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing steel and various corrosion-resistant alloys such as HUNTINGTON alloys G and 9041. It is useful for joining dissimilar metals involving INCONEL alloys, INCOLOY alloys, stainless steels, low-alloy and carbon steels. The weld metal has high strength at room and elevated temperatures and excellent corrosion resistance including resistance to pitting and crevice corrosion. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-313. Producer or source: Huntington Alloy Products Division, An INCO Company.