CANNON-MUSKEGON Nickel Alloy C is a cast nickel-base alloy with exceptionally high resistance to corrosion and with excellent high-temperature properties. It also has outstanding oxidation resistance and strength at elevated temperatures. Its many uses include heat-treating equipment, aerospace components and oil-refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Ni-255. Producer or source: Cannon-Muskegon Corporation.