PYROMET 31 is a nickel-base superalloy that exhibits an unusual combination of corrosion resistance and strength to temperatures as high as 1500 F (816 C). It has excellent resistance to hot sulfidation attack such as could occur in truck and locomotive diesel valve service. This datasheet provides information on composition, physical properties, and elasticity. Filing Code: Ni-252. Producer or source: Carpenter Technology Corporation.