Abstract

TECHALLOY WASPALOY, a nickel-base austenitic precipitation-hardenable alloy, derives its high strength at elevated temperatures from additions of the solid-solution strengthening elements molybdenum, cobalt and chromium and from aluminum and titanium which produce age hardening. Boron and zirconium additions also have been made to obtain optimum stress-rupture strength. It has excellent strength and good resistance to corrosion and oxidation at least to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-243. Producer or source: Techalloy Company Inc..