Abstract

FERRO-TIC DN-1 is comprised of a dispersion of extremely hard, inert titanium carbide grains in a special age-hardenable nickel-aluminum alloy matrix. It is characterized by excellent resistance to corrosion by strong chlorides. Its maximum operating temperature is 900 F. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as heat treating, machining, surface treatment, and powder metal forms. Filing Code: Ni-241. Producer or source: Chromalloy Metal Tectonics Company.