NIMAG 111 is a nickel-manganese alloy possessing good resistance to corrosion by sulfur compounds at elevated temperatures. It is recommended for such applications as electron tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-231. Producer or source: Spang Industries Inc..