Abstract

TRIBALOY T-700 consists of a hard, intermetallic phase in a softer, nickel-base matrix. It can be cast or hardfaced. As alloy powder it can be plasma sprayed or blended with other powders for P/M (Powder/Metallurgy) processing. It combines outstanding wear and corrosion resistance for use in pumps, extruders, bearings, mixers and particularly elements of nuclear reactors. It has excellent resistance to wear in liquid sodiium. This datasheet provides information on composition, physical properties, hardness, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion and wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: Ni-221. Producer or source: E. I. DuPont de Nemours & Company Inc..