Abstract

AMDRY 769 is a nickel-base alloy formulated to provide maximum resistance to abrasion, corrosion, heat and oxidation. It is deposited by spraying on the desired surface at a thickness usually limited to a maximum of 0.125 inch. The data pertain to the deposit after fusing. It has the same general usage as AMDRY 761 but thicker deposits can be made. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and powder metal forms. Filing Code: Ni-202. Producer or source: Alloy Metals Inc..

This content is only available as a PDF.
You do not currently have access to this content.