UNITEMP 718 is a nickel-base austenitic precipitation-hardenable alloy for extended service at temperatures up to 1200 F. For short periods the alloy performs well to about 1300 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-201. Producer or source: Cyclops Corporation.