Abstract

PYROTOOL 7 has been designed to display high tensile and yield properties with good hardness at temperatures up to 1300 F. It is used for high-temperature tooling, extrusion dies, forging dies, rams, mandrels, holders, rings, dummy blocks, liners, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-167. Producer or source: Carpenter Technology Corporation.