Pyromet 600 is a corrosion-resisting nickel-base alloy, having a very desirable combination of high strength and workability, both hot and cold. It has high strength and resistance to oxidation at high temperatures. It is designed to meet the highest quality of the nuclear industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-149. Producer or source: Carpenter Technology Corporation.