Abstract

NIKROTHAL LX is a nickel-chromium precision resistance alloy having a low temperature coefficient of resistance and a resistivity about three times that of copper-nickel type resistance alloys. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-148. Producer or source: The Kanthal Corporation. Originally published October 1969, revised February 1986.