Abstract

ALLOY 713LC is a nickel-base alloy possessing high stress-rupture strength up to 1700 F combined with excellent resistance to thermal fatigue. It is recommended for turbine wheels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-118. Producer or source: Austenal Microcast Division, Howmet Corporation.