Abstract

D-H No. 242 is a nickel-chromium high temperature alloy recommended for furnace components, heating elements and conveyor belts. It is also known as Nichrome V Def. #242. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-99. Producer or source: Driver-Harris Company.