Abstract

S Inconel is a nickel-base alloy recommended for applications requiring resistance to wear and galling in addition to high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-63. Producer or source: The International Nickel Company Inc..