INCONEL 600 nickel-base alloy has better high temperature properties than Inconel alloy, particularly where rupture strength, creep and short-time tensile are necessary. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-56. Producer or source: Huntington Alloy Products Division, An INCO Company.